Cuando un lote falla EN 1811: rechapado, reensayo y dónde está la línea de descarte
Short answer: Sometimes, but not on the same evidence. A failed EN 1811 batch can be stripped and re-plated when the nickel comes from the coating system itself: a nickel strike or underplate, a contaminated plating bath, or a coating that is too thin at an edge. It should be scrapped when the nickel sits ... <a title="When a Batch Fails EN 1811: Re-Plating, Retesting, and Where the Scrap Line Actually Is" class="read-more" href="https://amarajeweiry.com/es/en1811-failed-batch-replate-or-scrap/" aria-label="Leer más sobre When a Batch Fails EN 1811: Re-Plating, Retesting, and Where the Scrap Line Actually Is">Leer más</a>